A Study of Producing High Strength Concrete By using Silica Fume and Super Plasticizer

Show simple item record

dc.contributor.author Mohammed, zeinab Mustafa Suliman
dc.date.accessioned 2017-07-24T07:27:30Z
dc.date.available 2017-07-24T07:27:30Z
dc.date.issued 2017-05-10
dc.identifier.citation Mohammed, zeinab Mustafa Suliman . A Study of Producing High Strength Concrete By using Silica Fume and Super Plasticizer / zeinab Mustafa Suliman Mohammed ; Salih Elhadi Moh-Ahmed .- Khartoum: Sudan University of Science and Technology, College of Engineering Technology Industries, 2017 .- 84p. :ill. ;28cm .- M.Sc. en_US
dc.identifier.uri http://repository.sustech.edu/handle/123456789/18401
dc.description Thesis en_US
dc.description.abstract The aim of this study was to evaluate the performance of high strength Concrete (HSC) containing supplementary cementations materials (Silica Fume) and to find optimum range of silica fume content in the mix. In these study we prepared to tested some properties of high strength concrete 60 mpa in both fresh and hardened cases used slump test , compressive strength test and absorption test . The mix content silica fume in deferent percentage: 0.00%, 5.00%,10.00% and 15.00% replacement . 12 cube at each percentage tested at 3,7,28 days . Tested using local Sudanese aggregates with replacement (Silica Fume) and super plasticizers MCs 100 with 0.8%, 1%, 1.2% liter /100 kg c.m. Various percentages of silica fume (SF) were added at one water/cementations materials ratios (w/c.m). The methodology adopted to achieve the objectives of the research focuses mainly on a collection of data from different sources, an extensive review of previous studies, designing concrete mixes and implementing a lot of laboratory experiments using different ratios of silica fume and super plasticizer with low water contents. Ninety six of specimens were performed and 8 trial mix design of grade (60 MPa) HSC had been success fully produced and their mechanical properties were measured and documented. From these research we observed that the storage of silica fume has very important in final result ,whence silica fume replacement increases the slump test and compressive strength decreases as a result of bad storage en_US
dc.description.sponsorship Sudan University of Science and Technology en_US
dc.language.iso en en_US
dc.publisher Sudan University of Science and Technology en_US
dc.subject Construction Engineering en_US
dc.subject Super Plasticizer en_US
dc.subject High Strength Concrete en_US
dc.title A Study of Producing High Strength Concrete By using Silica Fume and Super Plasticizer en_US
dc.title.alternative دراسه حول إنتاج الخرسانة عالیة المقاومة بإستخدام غبار السیلیكا والملدنات en_US
dc.type Thesis en_US
dc.contributor.Supervisor Supervisor,- Salih Elhadi Moh-Ahmed