dc.contributor.authorEdreis, Maysa Elkheir Ali Sheik-
dc.contributor.authorSupervisor, -Khalid Mohammed Haroun-
dc.contributor.authorCo-Supervisor, -Ahmed Elhassan Alfaki-
dc.date.accessioned2022-04-11T07:05:58Z-
dc.date.available2022-04-11T07:05:58Z-
dc.date.issued2022-03-16-
dc.identifier.citationEdreis, Maysa Elkheir Ali Sheik .Effect of Doping Carbon Nanotubes with Magnesium Oxide on its Structural and Optical Properties and Used in Diode Multilayers \ Maysa Elkheir Ali Sheik Edreis ; Khalid Mohammed Haroun .- Khartoum:Sudan University of Science & Technology,College of Science,2022.- 96p.:ill.;28cm.-Ph.Den_US
dc.identifier.urihttp://repository.sustech.edu/handle/123456789/27156-
dc.descriptionThesisen_US
dc.description.abstractCarbon nanotube is long thin cylinders of graphite, it is made up of layers of carbon atoms every atom is connected evenly to three carbons arranged in a hexagonal lattice. In this research carbon nanotubes (CNTs) doping by magnesium oxide in different ratio (0.1, 0.3, 0.5, 0.7and 0.9) from soot and coal, were synthesized using thermal chemical vapour deposition (CVD), and used in diode Multilayers fabrication. Five samples of CNTs prepared from each source were doped by magnesium oxide in different ratio (0.1, 0.3, 0.5, 0.7and 0.9). X-ray diffraction technique (XRD) was used to obtain crystal structure and lattice parameters of samples, UV-Visible used to evaluate the optical properties.Fourier Transform Infrared spectroscopy (FTIR) used to measure the vibrational frequencies of bonds in the molecules. XRD results showed that the increasing in concentration of magnesium oxide leads to change structure parameter of carbon nanotubes samples (grain size, d-space, density and miller indices) FTIR showed different vibrational frequencies for CNTs from soot and coal, also showed that CNTs from coal more stable than CNTs from soot. For the optical properties the absorbance of CNTs from soot greater than CNTs from coal, for Soot samples the decrease of absorption at wavelengths 317 nm corresponding photon energy 3.912 eV by MgO concentration increase, and for Coal samples decrease at wavelengths 272 nm corresponding photon energy 4.559 eV by MgO concentration increase. The optical energy band gap decrease with MgO concentration increase, the optical band gap for soot and coal of CNTS within range of semiconductor materials (3.392-3.517) eV. Finally, the I-V Curve display that the samples are diode multilayer the charge injection voltage and turn off voltage increases when the concentration of MgO and number of layer increases for CNTS made from soot and coal. These results confirm the previous studies.en_US
dc.description.sponsorshipSudan University of Science & Technologyen_US
dc.language.isoenen_US
dc.publisherSudan University of Science & Technologyen_US
dc.subjectScienceen_US
dc.subjectPhysicsen_US
dc.subjectDoping Carbon Nanotubesen_US
dc.subjectMagnesium Oxideen_US
dc.subjectStructuralen_US
dc.subjectOptical Propertiesen_US
dc.subjectDiode Multilayersen_US
dc.titleEffect of Doping Carbon Nanotubes with Magnesium Oxide on its Structural and Optical Properties and Used in Diode Multilayersen_US
dc.title.alternativeأثر تشويب أنابيب الكربون النانوية بأوكسيد الماغنيسيوم على خصائصها التركيبية والضوئية واستخدامها كثنائي متعدد الطبقاتen_US
dc.typeThesisen_US
Appears in Collections:PhD theses : Science

Files in This Item:
File Description SizeFormat 
Effect of Doping Carbon ... .pdfResearch1.75 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.